Terylene tyre fabrics
terylene tyre fabrics specs table:
| Item |
1110dtex/2 (1000D/2) |
1110dtex/3 (1000D/3) |
| 8091 |
9091 |
10091 |
7491 |
8091 |
9091 |
| warp density(strand/cm) |
80±2 |
90±2 |
100±2 |
74±2 |
80±2 |
90±2 |
| zonal density(strand/10cm) |
8±1 |
8±1 |
8±1 |
8±1 |
8±1 |
8±1 |
| weft(cotton)tex |
10 |
10 |
10 |
10 |
10 |
10 |
| cloth breadth(cm) |
+1
91
-2 |
+1
91
-2 |
+1
91
-2 |
+1
91
-2 |
+1
91
-2 |
+1
91
-2 |
| cloth length(m) |
<(1+1%) |
<(1+1%) |
<(1+1%) |
<(1+1%) |
<(1+1%) |
<(1+1%) |
| odd bits of cloth |
strand |
5~7 |
5~7 |
5~7 |
5~7 |
5~7 |
5~7 |
| zonal density |
45~50 |
45~50 |
45~50 |
45~50 |
45~50 |
45~50 |
| length(cm) |
15~20 |
15~20 |
15~20 |
15~20 |
15~20 |
15~20 |
impregnation terylene tyre
fabrics:
|
Item |
1110dtex/2 |
1110dtex/3 |
| excellent |
first-class |
qualified |
excellent |
first-class |
qualified |
break strength
(N/strand) |
≥145 |
≥135 |
≥120 |
≥206 |
≥201 |
≥170 |
| fixed extension(%) |
4±1 |
4±1 |
4±1 |
4±1 |
4±1 |
4±1 |
adhesive strength
(N/cm) |
≥118 |
≥108 |
≥198 |
≥137 |
≥123 |
≥108 |
| break extension rate(%) |
12±2 |
12±2 |
12±2 |
13±2 |
13±2 |
13±2 |
| break strength uneven rate(%) |
≤3 |
≤4 |
≤5 |
≤3 |
≤4 |
≤5 |
| break extension uneven rate(%) |
≤4 |
≤5 |
≤6 |
≤4 |
≤5 |
≤6 |
| glue amount(%) |
5±1 |
5±1 |
5±1 |
5±1 |
5±1 |
5±1 |
| percentage of moisture(%) |
≤0.5 |
≤0.5 |
≤0.5 |
≤0.5 |
≤0.5 |
≤0.5 |
| twist degree(T/m) |
360/340
±15 |
360/340
±15 |
360/340
±15 |
340/340
±15 |
340/340
±15 |
340/340
±15 |
| Φ(mm) |
0.56±0.03 |
0.56±0.03 |
0.56±0.03 |
0.66±0.03 |
0.66±0.03 |
0.66±0.03 |
| dry-hot contractibility rate(%) |
≤4 |
≤4 |
≤4 |
≤4 |
≤4 |
≤4 |
For any special requirements on breadth and length,
it can be negotiated by two parties.
|
| |
address: Shidai one road, economic
development zone, Qingzhou city, Shandong province
Post Code: 262500
Tel:0536-3524066 3524099
Fax: 0536-2136278
E-mail: qzheli@163.com
qzheli1994@126.com
|